1. Chemical Composition of the products: C 0.70-1.20% Mn 0.60-1.20%, Si 0.40-1.20%, S≤0.05%, P ≤0.05%
2. Hardness: Normal: 40-50HRC Special: 52-56HRC, 56-60HRC Density: 7.4g/cucm
3. steel shot is used for industrial foundry, forging plant, heat treatment shop, steel construction plant, container manufacturer, ship builder, auto and locomotive manufacturer .
4. Microstructure: Tempered Marten site High strength, durable Ervin life: Cast steel shot: 2000 cycles